Technique: | Hot Rolled |
---|---|
Standard: | AISI, JIS, ASTM, DIN, BS, GB |
Grade: | (D2/1.2379/SKD11) |
Certificate: | ISO / Mill Certificate |
Test: | SGS / Ut 100% / Element Testing |
Payment: | 30% Deposit,Blance by L/C at Sight or T/T |
Customization: |
---|
Suppliers with verified business licenses
GB | AISI | DIN | JIS |
Cr12Mo1V1 | D2 | 1.2379 | SKD11 |
C | Si | Mn | S | P | Cr | Ni | Cu | V | Mo |
1.40-1.6 | 0.6 | 0.6 | 0.03 | 0.03 | 11.5-13 | 0.25 | 0.30 | 1.00 | 0.70 |
quench | temper | ||||||
Heating temperature/ºC | Cooling way | Hardness (HRC) | Tempering temperature /ºC |
Tempering number | Hardness (HRC) |
||
First preheating | Second preheating | Last heating | |||||
600-650 | 800-850 | 1020-1040 | Air Cooling | 61-63 | 500-560 | 2 | ≥58 |