Type: | Alloy Steel Bar |
---|---|
Standard: | AISI, ASTM, DIN, JIS, GB, BS |
Composition: | Alloy Steel |
Technique: | Hot Rolled |
Shape: | Round |
Surface Treatment: | Black |
Customization: |
---|
Suppliers with verified business licenses
C | Si | Mn | P | S | Cr |
0.18-0.23 | 0.25-0.30 | 070-0.90 | ≤0.025 | ≤0.025 | 1.30-1.65 |
Feature |
Demand has high yield strength, tensile strength and fatigue strength, there has enough plasticity and toughness; |
Demanding by refining outside the furnace, vacuum electroslag remelting or processing, or double vacuum smelting, vacuum induction furnace smelting suitable heat treatment; | |
Corrosion resistant steel, heat-resistant steel, wear-resistant steel, magnetic steel, and other special physical and chemical properties of the steel | |
Application | Zinc, aluminum, magnesium and other alloy die-casting molds |
Heat dies and all kinds of hot forged molds | |
Metal extrusion die holder | |
Heat Treatment |
Preheating 2-4 hours in 500-600°C |
Keeping temperature for 2 hours in 850-880°C | |
Oil cooling to reach 50-100°C | |
After quenching can reach a hardness of 50-5)2HRC, then tempered at 200°C, then hardness can reach above 48 HRC; | |
Melting Process | EAF:Electric Furnace+LF+VD(Optional) |
ESR:Electric Furnace+LF+VD+Eleroslag Remelted(Optional) | |
UT Class | According to Standard of SEP 1921/84,100% Volume, Level C/c, D/d or E/e |